| Data still to be completed------(<---links) | |
|---|---|
| PRODUCT DATA of CDA 762 | 
| Material | CDA 762 | 
| General Information | Typical data from standards handbook of copper and copper alloys (Copper.org) @ Room Temperature | 
| Chemical Composition | Cu-28.5Zn-12.2Ni | 
| EXPERIENCE IN PRACTICE | 
|---|
| Equivalent Designations | C76200; CuNi12Zn29; CW405J; CDA762 | 
| PHYSICAL PROPERTIES | 
|---|
| Specific Gravity | 8.58 | 
| ELASTIC PROPERTIES | 
|---|
| Tensile Modulus | 124 GPa | 
| Shear Modulus | 46.9 GPa | 
| ELECTRICAL PROPERTIES | 
|---|
| Electrical Volume Resistivity | 1.92e-7 ohm.m | 
| THERMAL PROPERTIES | 
|---|
| Thermal Conductivity | 45 W/m.K | 
| Thermal Expansion Coefficient | 16.2 µstrain/°C | 
| Melting Range | 980 to 1020 °C | 
| Specific Heat | 0.377 J/g.K | 
| RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY | 
|---|
| Stress Corrosion Status | Low Resistance to SCC: Table 3 Remark: in the annealed, 25% or 50% cold rolled condition only Remark: Requires Stress corrosion evaluation form Remark: acc. to ECSS-Q-ST-70-36C Data Quality: Design Data |