| Data still to be completed------(<---links) | |
|---|---|
| PRODUCT DATA of CDA 422 | 
| Material | CDA 422 | 
| General Information | Typical data from standards handbook of copper and copper alloys (Copper.org) @ Room Temperature | 
| Chemical Composition | Cu-12Zn-1Sn | 
| EXPERIENCE IN PRACTICE | 
|---|
| Equivalent Designations | CDA422 | 
| PHYSICAL PROPERTIES | 
|---|
| Specific Gravity | 8.8 | 
| ELASTIC PROPERTIES | 
|---|
| Tensile Modulus | 124 GPa | 
| ELECTRICAL PROPERTIES | 
|---|
| Electrical Volume Resistivity | 5.49e-8 ohm.m | 
| THERMAL PROPERTIES | 
|---|
| Thermal Conductivity | 130 W/m.K | 
| Melting Range | 1020 to 1040 °C | 
| Specific Heat | 0.377 J/g.K | 
| RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY | 
|---|
| Stress Corrosion Status | High Resistance to SCC: Table 1 Remark: in the 37% cold rolled condition only Remark: acc. to ECSS-Q-ST-70-36C Data Quality: Design Data |