| All data is for information only------(<---links) | |
|---|---|
| PRODUCT DATA of CDA 260 | 
| Material | CDA 260 | 
| General Information | Typical data from standards handbook of copper and copper alloys (CDA inc) @ Room Temperature | 
| Chemical Composition | Cu-30Zn | 
| EXPERIENCE IN PRACTICE | 
|---|
| Equivalent Designations | C26000; CuZn30; CW505L; 2.0265; CDA260; cartridge brass, 70%) | 
| PHYSICAL PROPERTIES | 
|---|
| Specific Gravity | 8.53 | 
| Magnetic Properties | Nonmagnetic | 
| ELASTIC PROPERTIES | 
|---|
| Tensile Modulus | 110 GPa | 
| Shear Modulus | 41.2 GPa | 
| ELECTRICAL PROPERTIES | 
|---|
| Electrical Volume Resistivity | 6.16e-8 ohm.m | 
| Electrical Conductivity | 28 %IACS | 
| THERMAL PROPERTIES | 
|---|
| Thermal Conductivity | 121 W/m.K | 
| Thermal Expansion Coefficient | 19.9 μstrain/°C | 
| Melting Range | 915 to 955 °C | 
| Specific Heat | 0.377 J/g.K | 
| RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY | 
|---|
| Stress Corrosion Status | Low Resistance to SCC: Table 3 Remark: in the 50% cold rolled condition only Not for primary structural items Remark: Requires Stress corrosion evaluation form Remark: acc. to ECSS-Q-ST-70-36C Data Quality: Design Data | 
| Welding | All welding processes | 
| SPECIAL RECOMMENDATIONS | 
|---|
| Special Recommendations | Alloy should be hot formed |