| PRODUCT DATA of CDA 172 | 
| Material | CDA 172 | 
| Precautions | Typical data work hardened/precipatation hardened Typical data from standards handbook of copper and copper alloys (Copper.org) @ Room Temperature | 
| CAS Registry Number | Cu-1.9Be | 
| EXPERIENCE IN PRACTICE | 
|---|
| Equivalent Designations | C17200; CUBE2; CW101C; 2.1247; CDA172; Beryllium-Copper 1.9% Be | 
| PHYSICAL PROPERTIES | 
|---|
| Specific Gravity | 8.26 | 
| ELECTRICAL PROPERTIES | 
|---|
| Electrical Volume Resistivity | 7.68e-8 ohm.m | 
| THERMAL PROPERTIES | 
|---|
| Thermal Conductivity | 107 W/m.K | 
| Thermal Expansion Coefficient | 18.8 μstrain/°C | 
| Melting Range | 866 to 982 °C | 
| Specific Heat | 0.419 J/g.K | 
| RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY | 
|---|
| Stress Corrosion Status | High Resistance to SCC: Table 1 Remark:High resistance only when solution treated/work hardened, then precipitation hardened. Data Quality: Design Data |