| Material | AA7020-T6 | 
| General Information | Heat treatable high strength weldable alloy. High fatigue strength. High strength in welded structures. | 
| EXPERIENCE IN PRACTICE | 
|---|
| Equivalent Designations | AA7005, AA 7005, AA 7020, AlZn4.5Mg1, A-Z5G, 3.4335, D74S | 
| PHYSICAL PROPERTIES | 
|---|
| Crystal Structure | Face centered cubic (fcc) | 
| Specific Gravity | 2.78 | 
| Magnetic Properties | Nonmagnetic | 
| ELASTIC PROPERTIES | 
|---|
| Tensile Modulus | 70 GPa | 
| Shear Modulus | 26.4 GPa | 
| THERMAL PROPERTIES | 
|---|
| Thermal Conductivity | 140 W/m.K | 
| Thermal Expansion Coefficient | 23.3 µstrain/°C | 
| Melting Range | 605 to 645 °C | 
| Specific Heat | 0.873 J/g.K | 
| RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY | 
|---|
| General Corrosion Status | Requires specific corrosion protection | 
| Stress Corrosion Status | Low Resistance to SCC: Table 3 Remark:Including weldments Data Quality: Design Data | 
| Bimetallic Corrosion | Can be used in a non-controlled environment: Al alloys, Cd Can be used in a clean room environment: Mg, Sn-Pb alloys (all), Sn, Pb, Zn, Be Needs specific measures: All others Test: ECSS-Q-ST-70C Rev.1 Table 5.1 Data Quality: Design Data |