OUTGASSING DATA of POLYURETHANE COATED KEVLAR LANYARD KST-0-CL
Manufacturer
WESTERN FILAMENT
Product_Type
LACING TAPE
Result
TML=3.30%; RML=1.30%; CVCM=0.22%
Reference
GSC33298 / 2013 / NASA Outgassing database