OUTGASSING DATA of TEMP-R-TAPE G-565 FIBERGLASS/SILICONE ADH/F FLAME R
ManufacturerFuron
Product_TypeTAPE
ResultTML=2.72%; RML=2.72%; CVCM=1.46%
ReferenceGSC13183 / 1983 / NASA Outgassing database