PRODUCT DATA of ZK60A |
Material | ZK60A |
General Information | ZK60A is a heat treatable magnesium alloy used primarily in extruded shapes and forgings. Given data for T5 and T6 condition |
Chemical Composition | Mg-Zn5.5%, Zr0.45% |
EXPERIENCE IN PRACTICE |
---|
Equivalent Designations | UNS M16600 |
PHYSICAL PROPERTIES |
---|
Specific Gravity | 1.83 |
Magnetic Properties | Nonmagnetic |
ELASTIC PROPERTIES |
---|
Tensile Modulus | 45 GPa |
Shear Modulus | 17 GPa |
Poisson Ratio | 0.35 |
THERMAL PROPERTIES |
---|
Thermal Conductivity | 121 W/m.K |
Thermal Expansion Coefficient | 27 μstrain/°C |
Specific Heat | 1.1 J/g.K |
Melting Range | 520 to 635 °C |
RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY |
---|
General Corrosion Status | Requires specific corrosion protection |
Stress Corrosion Status | Moderate Resistance to SCC: Table 2
Remark:Requires Stress corrosion evaluation form Remark: acc. to ECSS-Q-ST-70-36C Data Quality: Design Data |
Bimetallic Corrosion | Can be connected in a clean room environment to: Sn-Pb alloys, Sn, Pb Needs specific measures: All others
Data Quality: Design Data |