PRODUCT DATA of H-11 |
Material | H-11 |
Chemical Composition | Fe-0.40% C, 1.05% Si, 5.00% Cr, 1.35% Mo, 0.35% V |
EXPERIENCE IN PRACTICE |
---|
Development Status | Commercial Product |
PHYSICAL PROPERTIES |
---|
Specific Gravity | 7.8 |
ELASTIC PROPERTIES |
---|
Tensile Modulus | 200 GPa |
Shear Modulus | 81 GPa |
Bulk Modulus | 140 GPa |
Poisson Ratio | 0.3 |
THERMAL PROPERTIES |
---|
Thermal Conductivity | 24.6 W/m.K |
Thermal Expansion Coefficient | 11 μstrain/°C |
Specific Heat | 0.46 J/g.K |
RELEVANT PROPERTIES FOR USE IN SPACE COMMUNITY |
---|
Stress Corrosion Status | High Resistance to SCC: Table 1: UTS below 1450 MPa Low Resistance to SCC: Table 3: UTS above 1450 MPa UTS Remark: acc. to ECSS-Q-ST-70-36C Data Quality: Design Data |
Machinability | Machinability is reasonably good, approximately 75% water hardening low alloy tool steels. |
Welding | H11 is a readily weldable alloy by conventional methods. |