Data still to be completed------(Home) | |
---|---|
PRODUCT DATA of CDA 745 |
Material | CDA 745 |
General Information | Typical data from standards handbook of copper and copper alloys (CDA inc) @ Room Temperature |
Chemical Composition | Cu-10Ni-25Zn |
EXPERIENCE IN PRACTICE |
---|
Development Status | Commercial Product |
Equivalent Designations | CDA745; Nickel-Silver 65-10 |
PHYSICAL PROPERTIES |
---|
Specific Gravity | 8.69 |
ELASTIC PROPERTIES |
---|
Tensile Modulus | 121 GPa |
Shear Modulus | 45.1 GPa |
ELECTRICAL PROPERTIES |
---|
Electrical Volume Resistivity | 1.92e-7 ohm.m |
THERMAL PROPERTIES |
---|
Thermal Conductivity | 46.1 W/m.K |
Thermal Expansion Coefficient | 16.4 µstrain/°C |
Specific Heat | 0.377 J/g.K |